@equivestinvest Pyrite has been a curse for punters over many decades - fool's gold, fool's copper and now fool's nickel
@ChuckChunder007 @equivestinvest could the melting point of pyrite at 1200C vs nickel sulfides at 800C explain why the pyrite is more superficial? Or it doesn't work like that? @equivestinvest
@ChuckChunder007 @equivestinvest especially since this is the edge of the anomaly. pyrite solidifies first, leaving molten nickel sulfide towards the middle and lower in the ground.